MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F263 Epoxy Resin, T3T190 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: T_190-12"-F263; Various fibers

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 55.0 %55.0 %Laminate Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 1353 MPa
@Temperature 24.0 °C
196200 psi
@Temperature 75.2 °F
Tensile Modulus 131.8 GPa
@Temperature 24.0 °C
19120 ksi
@Temperature 75.2 °F
Compressive Yield Strength  1185 MPa
@Temperature 71.0 °C
171900 psi
@Temperature 160 °F
 1212 MPa
@Temperature 24.0 °C
175800 psi
@Temperature 75.2 °F
Shear Strength  76.0 MPa
@Temperature 132 °C
11000 psi
@Temperature 270 °F
Short Beam
 110 MPa
@Temperature 24.0 °C
16000 psi
@Temperature 75.2 °F
Short Beam
 122 MPa
@Temperature -54.0 °C
17700 psi
@Temperature -65.2 °F
Short Beam
 
Descriptive Properties
Cured Thickness per Ply (cm)0.02Laminate
Dry Resin Content (%)35-39Prepreg
Flow (%)11-24

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
Hexcel® HexMC® C / 2000 / R1 Composite SMC
Hexcel® Fibrelam® 2000 Grade 5 Panels for Aircraft Flooring
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring
Goodfellow Carbon-Carbon Composite

PHEXC123 / 98593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.