Moplen HP420J is a polypropylene homopolymer manufactured using the Spheripol process. It is particularly suitable for BOPP, with potential end use applications in general purpose packaging, lamination film and adhesive tape. Applications: Food Packaging Film, Lamination FilmInformation provided by LyondellBasell. |