MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Hicast HT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Calcined chamotte / Bauxite. Hydraulic bond. A low cement, chamotte - bauxite 1650°C castable with high strengths at all temperatures, low porosity and excellent abrasion, impact and alkali resistance.

Applications:

  • Forge furnace hearths
  • Door jambs, lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and dams
  • Rotary hearth curbs
  • Walking beam furnace hearth, pusher furnace hearths
  • Skid pipe protection

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.53 g/cc0.0914 lb/in³dried to 110°C
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  75.0 MPa
@Treatment Temp. 110 °C
10900 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 85.0 MPa
@Treatment Temp. 815 °C
12300 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 95.0 MPa
@Treatment Temp. 1000 °C
13800 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 110 MPa
@Treatment Temp. 1600 °C
16000 psi
@Treatment Temp. 2910 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.83 W/m-K
@Temperature 600 °C
12.7 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1650 °C<= 3000 °F
Shrinkage  -1.50 - 1.5 %
@Treatment Temp. 1600 °C
-1.50 - 1.5 %
@Treatment Temp. 2910 °F
 0.00 - 0.20 %
@Treatment Temp. 110 °C
0.00 - 0.20 %
@Treatment Temp. 230 °F
 0.20 %
@Treatment Temp. 815 °C
0.20 %
@Treatment Temp. 1500 °F
 0.30 %
@Treatment Temp. 1000 °C
0.30 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 67 %67 %
CaO 1.7 %1.7 %
Fe2O3 1.0 %1.0 %
K2O+Na2O 0.20 %0.20 %Na2O+ K2O
MgO 0.10 %0.10 %
SiO2 27 %27 %
TiO2 2.1 %2.1 %
 
Descriptive Properties
Net Material Required (kg/m³)2530
Water Addition5.5-6.5 % by weight, 1..375-1.635 L per bag, 25 Kg bag weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6278 / 203062

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.