MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials VTR 8550 (GFLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: VTR-8550 is 67% fluorine peroxide cured polymer similar to Viton® GFLT with significantly improved processing and curing characteristics. VTR-8550 utilizes an Advanced Polymer Architecture technology designed to deliver a polymer which:
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to GFLT or GFLT-300
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell in a ~60 Mooney FKM
  • Shows excellent physical properties with high elongation in either the original or aging tests
  • Shows similar to improved heat, fluids, and low temperature resistance compared to GFLT
  • Shows excellent compression set resistance with little (2 hr at 232°C) or no postcure

It is recommended to use at least a 70% load factor in an internal mixer. The recommended process aid for VTR-8550 is 0.5 phr of Armeen® 18D. A two part process aid system of Armeen® 18D with Strucktol WS 280 at 0.8 phr each is optimal if that level of process aid can be tolerated in mold shrinkage. The use of Diak™ #8 is NOT recommended as it causes poor mold release and high compression set.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 64
@Temperature 121 °C
ML-10 (gum)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 18.3 MPaCured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Yield 0.000800 GPa10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 207 %Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00660 GPa
@Strain 100 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 11 %
@Temperature 200 °C
Method B, O-rings 22 hr at 200°C (Post Cured 2 hr at 232°C)
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -23.9 °CTR-10
Glass Transition Temp, Tg -25.7 °CDSC
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 67 %
 
Descriptive Properties
Formulation as Tested100VTR-8550
 3Zinc Oxide
 3Diak™ 7 (TAIC)
 3Luperox® 101-XL 45
 30N990 Carbon Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation
Seals Eastern 5724 Fluorocarbon-Elastomer
Chemours Viton® F-605C Fluoroelastomer (FKM)
Chemours Viton® ETP-900 Fluoroelastomer (FKM)
DuPont Mobility and Materials GLT305 Peroxide Cured Fluoroelastomer (FKM) Formulation

PDVDA51 / 34020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.