MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Jilin Xingyun Chemical YY-1010 Antioxidant
Categories: Other Engineering Material

Material Notes: The product of Antioxidant YZ-1010 is not only the a antioxidant of multivariate hindered phenol, but also abroad –spectrum plastic additive with high efficiency, low toxicity, non-pollution, which is soluble in benzene, acetone, chloroform and other organic solvents, slightly soluble in ethanol, and insoluble in water, showing the performance of resistance to thermal water and good detergent extraction, low volatility, good compatibility with majority polymers, and excellent thermal stability and anti thermal aging oxidation. The product can protect the material from damages due to heat oxidation, widely used in PE, PS, ABS resin, polyurethane, PBT, PVC, polyoxymethylene, polyamide, and various synthetic rubber and other polymer materials.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 125 °C230 - 257 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 96 %
@Wavelength 425 nm
>= 96 %
@Wavelength 425 nm
2g/20ml toluene
 >= 98 %
@Wavelength 500 nm
>= 98 %
@Wavelength 500 nm
2g/20ml toluene
 
Descriptive Properties
AppearanceWhite or slightly yellow crystalline powder
Content=98%Effective component
 >94%Main

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJILINX033 / 317880

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.