Moplen HP456J is a polypropylene homopolymer used for extrusion and thermoforming applications. Moplen HP456J is formulated with a low water-carry-over additive package. Typical applications are monofilaments, ropes and tapes. Applications: Raffia/Tapes/Strapping.Information provided by LyondellBasell. |