MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and high quality SEBS compounds. It is polyolefin-based and UV stable. Supplied as free-flowing pellets in 20 kilogram (44 pound) moisture barrier bags.

Features:

  • Water used as physical foaming agent
  • Density range 0.95 to 0.15 depending on foaming agent
  • Excellent ozone resistance

Product Notes: Values are for injection molded plaques, side gated.
82.6 mm x 117.5 mm x 3 mm

Information provided by Advanced Elastomer Systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 755 seconds; ASTM D2240
 8015 seconds; ASTM D2240
 8015 seconds, After oven air aging 1008 hrs. @ 125°C; ASTM D2240
Tensile Strength at Break 1215 psiAfter oven air aging 1008 hrs. @ 125°C; ASTM D412
 1350 psiAcross flow; ASTM D412
Tensile Stress at Strain 490 psi
@Strain 100 %
across flow; ASTM D412
Elongation at Break 504 %After oven air aging 1008 hrs. @ 125°C; ASTM D412
 560 %Across flow; ASTM D412
Compression Set 44 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; ASTM D395
 46 %
@Temperature 236 °C,
Time 252000 sec
Method B; ASTM D395
Tensile Set 11 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -58.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 - 232 °C
Drying Temperature 82.0 °CDesiccant Dryer
Dry Time 3 hourDesiccant Dryer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber

PADW153 / 22871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.