Physical Properties | Original Value | Comments |
---|
Density | 1.24 g/cc |
Moisture Absorption | 0.80 - 0.90 % @Temperature 70.0 °C |
Water Absorption at Saturation | 2.2 % |
Linear Mold Shrinkage, Flow | 0.018 cm/cm |
Linear Mold Shrinkage, Transverse | 0.021 cm/cm |
Spiral Flow | 58.0 cm |
|
Mechanical Properties | Original Value | Comments |
---|
Tensile Strength, Yield | 60.0 MPa |
| 12.0 MPa @Temperature 80.0 °C |
| 16.2 MPa @Temperature 80.0 °C |
| 16.8 MPa @Temperature 80.0 °C |
| 18.0 MPa @Temperature 80.0 °C |
| 18.0 MPa @Temperature 80.0 °C |
| 40.8 MPa @Temperature 23.0 °C |
| 52.8 MPa @Temperature 23.0 °C |
| 53.4 MPa @Temperature 23.0 °C |
| 53.4 MPa @Temperature 23.0 °C |
| 54.0 MPa @Temperature 120 °C |
| 54.0 MPa @Temperature 80.0 °C |
| 54.0 MPa @Temperature 23.0 °C |
| 55.2 MPa @Temperature 45.0 °C |
| 55.2 MPa @Temperature 23.0 °C |
| 55.2 MPa @Temperature 23.0 °C |
| 56.4 MPa @Temperature 23.0 °C |
| 57.0 MPa @Temperature 23.0 °C |
| 57.6 MPa @Temperature 23.0 °C |
| 57.6 MPa @Temperature 23.0 °C |
| 63.6 MPa @Temperature 120 °C |
| 63.6 MPa @Temperature 80.0 °C |
| 64.8 MPa @Temperature 45.0 °C |
| 65.4 MPa @Temperature 45.0 °C |
| 66.0 MPa @Temperature 120 °C |
| 66.0 MPa @Temperature 80.0 °C |
| 66.6 MPa @Temperature 45.0 °C |
| 68.4 MPa @Temperature 80.0 °C |
| 69.0 MPa @Temperature 80.0 °C |
| 72.6 MPa @Temperature 80.0 °C |
| 72.6 MPa @Temperature 80.0 °C |
Elongation at Break | >= 300 % |
Tensile Modulus | 1400 MPa |
Flexural Strength | 60.0 MPa |
Flexural Modulus | 1600 MPa |
Charpy Impact Unnotched | NB @Temperature 23.0 °C |
| NB @Temperature -30.0 °C |
Charpy Impact, Notched | 4.50 kJ/m² @Temperature -30.0 °C |
| 15.0 kJ/m² @Temperature 23.0 °C |
Coefficient of Friction, Dynamic | 0.52 |
K (wear) Factor | 34.0 x 10-8 mm³/N-M |
|
Electrical Properties | Original Value | Comments |
---|
Volume Resistivity | 1.00e+13 ohm-cm |
Surface Resistance | 1.00e+13 ohm |
|
Thermal Properties | Original Value | Comments |
---|
Melting Point | 220 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C |
Flammability, UL94 | HB @Thickness 1.60 mm |
|
Processing Properties | Original Value | Comments |
---|
Feed Temperature | 60.0 - 80.0 °C |
Nozzle Temperature | 230 - 250 °C |
Zone 1 | 210 - 250 °C |
Zone 2 | 210 - 250 °C |
Zone 3 | 210 - 250 °C |
Zone 4 | 210 - 250 °C |
Melt Temperature | 230 - 250 °C |
Mold Temperature | 60.0 - 80.0 °C |
Drying Temperature | 60.0 - 80.0 °C |
Dry Time | <= 4.00 hour |
Back Pressure | 30.0 - 80.0 MPa |
|
Descriptive Properties |
---|
Resistance to Acetic Acid | 1% Change in Volume |
| 1% Change in Volume |
| 3% Change in Weight |
| 3% Change in Weight |
Resistance to Acetone | 2% Change in Volume |
| 5% Change in Volume |
| 5% Change in Weight |
| 5% Change in Weight |
Resistance to Ammonium hydroxide 10% | 0% Change in Volume |
| 0% Change in Weight |
| -3% Change in Volume |
| -5% Change in Weight |
Resistance to Antifreeze 50%, 50% water | 0% Change in Volume |
| 0% Change in Weight |
| 1% Change in Volume |
| 1% Change in Weight |
Resistance to Antifreeze, 100% ethylene glycol | 0% Change in Volume |
| 0% Change in Weight |
| 5% Change in Volume |
| 5% Change in Weight |
Resistance to Automatic transmission fluid | 0% Change in Volume |
| 0% Change in Volume |
| 0% Change in Weight |
| 0% Change in Weight |
Resistance to Brake fluid | 0% Change in Volume |
| 0% Change in Weight |
| 5% Change in Volume |
| 5% Change in Weight |
Resistance to Butyl acetate | 0% Change in Volume |
| 0% Change in Weight |
| 2% Change in Volume |
| 2% Change in Weight |
Resistance to Calcium Chloride | 0% Change in Volume |
| 0% Change in Weight |
Resistance to Chassis lube | 0% Change in Volume |
| 0% Change in Weight |
| -1% Change in Volume |
| -1% Change in Weight |
Resistance to Dichloroethane | 0% Change in Volume |
| 0% Change in Weight |
Resistance to Dimethyl formamide | 0% Change in Volume |
| 2% Change in Weight |
| Samples swell and slowly dissolve |
| Samples swell and slowly dissolve |
Resistance to Ethanol | 1% Change in Volume |
| 2% Change in Volume |
| 2% Change in Weight |
| 2% Change in Weight |
Resistance to Gasohol (unleaded, 10% methanol) | 0% Change in Volume |
| 1% Change in Weight |
| 3% Change in Weight |
| 5% Change in Volume |
Resistance to Gasohol M-25 (unleaded, 15% methanol) | 0% Change in Volume |
| 1% Change in Weight |
| 3% Change in Volume |
| 5% Change in Weight |
Resistance to Heptane | 0% Change in Volume |
| 0% Change in Volume |
| 0% Change in Weight |
| 0% Change in Weight |
Resistance to Hydraulic fluid | 0% Change in Volume |
| 0% Change in Volume |
| 0% Change in Weight |
| 0% Change in Weight |
Resistance to Hydrochloric acid | 0% change in volume |
| 0% change in volume |
| 2% change in weight |
| 2% change in weight |
Resistance to Jet fuel A | 0% Change in Volume |
| 0% Change in Weight |
| 1% Change in Weight |
| 2% Change in Volume |
Resistance to Methanol | 1% Change in Volume |
| 2% Change in Weight |
| 2% Change in Weight |
| 3% Change in Volume |
Resistance to Methylethylketone | 2% Change in Volume |
| 2% Change in Weight |
Resistance to Motor oil (SAE 10W-40) | 0% Change in Volume |
| 0% Change in Weight |
| 0% Change in Weight |
| -1% Change in Volume |
Resistance to MTBE | 1% Change in Volume |
| 1% Change in Weight |
Resistance to Sodium Chloride 10% | 0% Change in Volume |
| 0% Change in Weight |
| 0% Change in Weight |
| -1% Change in Volume |
Resistance to Sodium hydroxide 10% | 0% Change in Volume |
| 1% Change in Weight |
| 5% Change in Volume |
| 5% Change in Weight |
Resistance to Sodium hypochlorite 4.6% | -1% Change in Volume |
| -1% Change in Volume |
| -1% Change in Weight |
| -2% Change in Weight |
Resistance to Sulfuric acid | 0% change in volume |
| 0% change in volume |
| 0% change in weight |
| -1% change in volume |
| -1% change in volume |
| 1% change in weight |
| -1% change in weight |
| -1% change in weight |
Resistance to Tetrachloroethylene | 0% Change in Volume |
| 1% Change in Weight |
| 2% Change in Volume |
| 3% Change in Weight |
Resistance to Toluene | 0% Change in Volume |
| 1% Change in Volume |
| 1% Change in Weight |
| 4% Change in Weight |
Resistance to Trichlorethane | 0% Change in Volume |
| 1% Change in Volume |
| 1% Change in Weight |
| 5% Change in Weight |
Resistance to Unleaded gasoline | 0% Change in Volume |
| 0% Change in Weight |
| 1% Change in Weight |
| 3% Change in Volume |
Resistance to Xylene | 0% Change in Volume |
| 0% Change in Weight |
Resistance to Zinc chloride 10% | 2% Change in Weight |
| 3% Change in Volume |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.