MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Trinseo Magnum™ 780HP ABS, High Heat, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

MAGNUM® 780HP ABS resin is a low gloss, high heat, high impact grade designed for use in small household appliances. It offers a good balance of physical properties and excellent injection molding characteristics.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108
Tensile Strength, Yield 44.8 MPaASTM Data
Elongation at Yield 2.5 %ISO Data
Tensile Modulus 2.07 GPaASTM Data
Izod Impact, Notched 2.40 J/cmASTM Data
Charpy Impact Unnotched NBISO Data
 NBISO Data, Low Temp
Charpy Impact, Notched 0.700 J/cm²ISO Data, Low Temp
 2.00 J/cm²ISO Data
Instrumented Impact Total Energy 45.0 J
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 78.0 µm/m-°C
@Temperature 20.0 °C
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CUnannealed; 103°C (217°F) annealed; ASTM Data
Vicat Softening Point 111 °C
 
Optical PropertiesOriginal ValueComments
Gloss 52.5 %Gardner Gloss, 60°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 758HP ABS, High Heat, High Impact
Trinseo Magnum™ 358HP ABS, High Heat
A. Schulman LPP10BK38BK 10% Calcium Carbonate Filled, Heat-Stabilized, Impact Modified Polypropylene
A. Schulman Gapex® RPP30EA20HB 30% Fiberglass Reinforced, Chemically-Coupled, Heat Stabilized, Homopolymer Polypropylene
A. Schulman Ferrex® GPP20CS70BK 20% Calcium Carbonate Filled, Heat-Stabilized, Impact Modified Polypropylene containing 25% P.C.R.

PZZDW097 / 34328

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.