MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUTENE FB0800 LDPE Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical properties and optical properties make suitable for manufacture of greenhouse films. (LUTENE FB0800 contains slip agent and

Main Application: Greenhouse, tunnel film, film

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.921 g/cc0.921 g/ccASTM D1505
Water Vapor Transmission 12.0 g/m²/day0.773 g/100 in²/day
Oxygen Transmission Rate 2000 cc/m²/day129 cc/100 in²/day
Nitrogen Transmission 3500 cc-mm/m²-24hr-atm8890 cc-mil/100 in²-24hr-atm
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 650 %650 %ASTM D882
Elmendorf Tear Strength MD 280 g280 gASTM D1922
Elmendorf Tear Strength TD 350 g350 gASTM D1922
Dart Drop Test 230 g0.507 lbASTM D1709
Film Tensile Strength at Break, MD 21.7 MPa3150 psiASTM D882
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °FDSC
Vicat Softening Point 94.0 °C201 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 200 °C338 - 392 °F
Blow-up Ratio (BUR) 1.5 - 2.01.5 - 2.0
 
Descriptive Properties
Slip Coefficient0.15ASMT D1894

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2540D Low Density Polyethylene
Versalis Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion
FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene
Braskem Green PE SGM7746C Blow Molding and Monofilament High Density Polyethylene

PLAY214 / 148224

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.