MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6 GF 10 FRG 5 Polyamide 6, 10% Glass Fiber, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 10% glass fiber. Application: impacted mouldings with high strength applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears, cases of the electrotools, coolings screws of blowers, electromotors, carrying parts in the automotive industry. With the increasing content of GF also the toughness, bending and tensile strength increase as well as the heat application increases up to 150°C and the shrinkage decreases. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0054 cm/cm0.0054 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0078 cm/cm0.0078 in/inSTN 64 0808
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiSTN EN ISO 527-2
Elongation at Break 4.0 %4.0 %STN EN ISO 527-2
Tensile Modulus 5.95 GPa863 ksiSTN EN ISO 527-2
Flexural Strength 172 MPa24900 psiSTN EN ISO 178
Flexural Modulus 4.75 GPa689 ksiSTN EN ISO 178
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -20.0 °C
23.8 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.700 J/cm²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDSC; STN EN ISO 3146
Vicat Softening Point 250 °C482 °FB; STN EN ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Test 960 °C1760 °F3mm; STN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.20 %0.20 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced
Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength

PPLACO029 / 106907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.