MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.

Available in: Europe

Product Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is recommended for mechanical components which require a very good surface finish with low warpage, and good compression strength. This product is available in natural, black, and in special colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183/A
Water Absorption 0.70 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.014 cm/cm
Linear Mold Shrinkage, Transverse 0.014 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPaISO 527 Type 1A
Elongation at Break 15 %ISO 527 Type 1A
Elongation at Yield 4.0 %ISO 527 type 1 A
Tensile Modulus 5000 MPaISO 527 Type 1A
Flexural Strength 150 MPaISO 178
Flexural Modulus 4700 MPaISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 19.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+14 ohm-cmIEC 60093
Surface Resistance 5.00e+14 ohmIEC 60093
Dielectric Strength 28.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 500 VSolution B; IEC 60112
 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A218 Heat Stabilized Nylon 66
Domo TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Domo Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Domo Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0

PRHOD598 / 137829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.