MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical Lupoy 1320C-07 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Description: LUPOY PC 1320C-07 resin provides stability against ultraviolet radiations to solid or multi-wall sheets via the coextrusion of a 50 ? thick layer

Main Characteristics: Proprietary formulation, Very low plate-out characteristics, Very high thermal stability and Very good color stability

Applications: UV layer coating and Master batch

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.0 MPa9860 psi50mm/min; ASTM D638
Elongation at Break 113 %113 %50mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50mm/min; ASTM D638
Tensile Modulus 2.00 GPa290 ksi1mm/min; ASTM D638
Flexural Strength 68.0 MPa9860 psi50mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi)  130 °C
@Thickness 4.00 mm
266 °F
@Thickness 0.157 in
Annealed; ASTM D648
 133 °C
@Thickness 4.00 mm
271 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Vicat Softening Point 138 °C
@Load 5.10 kg
280 °F
@Load 11.2 lb
50°C/hr; ASTM D1525
Flash Point >= 450 °C>= 842 °F
Ignition Temperature >= 450 °C>= 842 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 0.70 - 1.5 %0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1201-08 Polycarbonate Resin
LG Chemical Lupoy 1200-08 Polycarbonate Resin
LG Chemical LUPOY HI1002ML PC, High Impact
LG Chemical Lupoy 1603-06 Polycarbonate Resin
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin

PLAY665 / 148675

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.