Ultrasint® PP nat 01 now harnesses the properties of polyolefins for PBF technologies, delivering the well-known characteristics of polypropylene, such as excellent chemical resistance, ductility and media tightness. Highlights: - Excellent plasticity
- High elongation
- Low moisture absorption
- High durability
Applications: - Pipes and ducts for and other media
- Water reservoirs and manifolds
- Economic and functional prototypes
- Multi-purpose industrial goods
- Durable jigs and fixtures
Information provided by Advanced Laser Materials |