MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SACO AEI PEXIDAN® L/T Red/White/Blue Curable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® L/T (including L/T-UV and L/T Eclipse) is a high density PEX system consisting of a silane grafted base compound A-1001 and a catalyst masterbatch CAT-003 (or A-1022 and CAT-117). When mixed and extruded in the proper proportions, the two-component system results in a material that is crosslinkable by exposure to moisture or by immersion in hot water at 90-95°C. PEXIDAN® L/T is listed by NSF International to standards 14 and 61 and to Canadian Standards Association standard B137.5. NSFI certification to ASTM F876 and ASTM F2023 testifies to its superior resistance to oxidation by hot, chlorinated water. PEXIDAN® L/T is permitted to be used in domestic continuous re-circulation systems and is listed by NSF as a NSF-pw CL5 / PEX 5006 material.

Typical values reported above (except MFR) are obtained from samples cured in hot water (6 hours @ 95°C).

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.946 g/cc0.946 g/ccASTM D792
Oxidative Induction Time (OIT) >= 50 min
@Temperature 220 °C
>= 50 min
@Temperature 428 °F
ASTM D3895
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature <= -1.11 °C<= 30.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.61 MPa3425 psiASTM D638
 12.0 MPa
@Temperature 82.0 °C
1740 psi
@Temperature 180 °F
ASTM D638
 12.0 MPa
@Temperature 93.0 °C
1740 psi
@Temperature 199 °F
ASTM D638
Tensile Strength, Yield 21.4 MPa3100 psiASTM D638
 8.69 MPa
@Temperature 93.0 °C
1260 psi
@Temperature 199 °F
ASTM D638
 11.20 MPa
@Temperature 82.0 °C
1625 psi
@Temperature 180 °F
ASTM D638
Elongation at Break 0.00 %0.00 %Hot, Permanent elongation (set) after cooling; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 240 %240 %ASTM D638
 200 %
@Temperature 82.0 °C
200 %
@Temperature 180 °F
ASTM D638
 240 %
@Temperature 93.0 °C
240 %
@Temperature 199 °F
ASTM D638
 30 %
@Temperature 150 °C,
Time 900 sec
30 %
@Temperature 302 °F,
Time 0.250 hour
Hot, Elongation under 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
Elongation at Yield 9.0 %9.0 %ASTM D638
 12 %
@Temperature 82.0 °C
12 %
@Temperature 180 °F
ASTM D638
 14 %
@Temperature 93.0 °C
14 %
@Temperature 199 °F
ASTM D638
Tensile Modulus  0.862 GPa
@Temperature 23.0 °C
125 ksi
@Temperature 73.4 °F
ISO 527
 1.69 GPa
@Temperature 0.000 °C
245 ksi
@Temperature 32.0 °F
ISO 527
 2.31 GPa
@Temperature -40.0 °C
335 ksi
@Temperature -40.0 °F
ISO 527
Flexural Modulus  0.207 GPa
@Temperature 23.0 °C
30.0 ksi
@Temperature 73.4 °F
elastic; ISO 178
 0.379 GPa
@Temperature 0.000 °C
55.0 ksi
@Temperature 32.0 °F
elastic; ISO 178
 0.517 GPa
@Temperature -40.0 °C
75.0 ksi
@Temperature -40.0 °F
elastic; ISO 178
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature -100 - 85.0 °C
83.3 µin/in-°F
@Temperature -148 - 185 °F
ASTM D696
Specific Heat Capacity 1.92 J/g-°C0.459 BTU/lb-°F
Vicat Softening Point 124 °C255 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 177 °C320 - 350 °Fbarrel zones
Die Temperature 185 °C365 °F
Head Temperature 185 °C365 °F
 
Descriptive Properties
Degree of Crosslinking70%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO046 / 249413

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.