TEB is a co-catalyst product soluble in aromatic and saturated aliphatic and cycloaliphatic hydrocarbons. Used in a chromium catalyst system. CAS number: 97-94-9 EINECS/ELINCS No.: 202-620-9 Applications: TEB may be used in organic synthesis as an agent for stereochemical control. TEB is also used as an adjuvant for Ziegler- Natta and silica-supported chromium catalysts for olefin polymerization. Information provided by Nouryon |