MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
3013-O Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A93013; Aluminium 3013; AA3013; Al3013-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.74 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 29
Tensile Strength, Ultimate 105 MPa
Tensile Strength, Yield 45.0 MPa0.2% offset
Elongation at Break 29 %
Modulus of Elasticity 68.9 GPaAA3004 - Average of tension and compression
Poissons Ratio 0.35AA3004
Shear Modulus 25.0 GPaAA3004
Shear Strength 70.0 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000416 ohm-cmAA3004
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.2 µm/m-°C
@Temperature 20.0 - 100 °C
AA3004
Specific Heat Capacity 0.893 J/g-°CAA3004
Thermal Conductivity 163 W/m-KAA3004
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 94.7 - 98.4 %As remainder
Copper, Cu <= 0.50 %
Iron, Fe <= 1.0 %
Magnesium, Mg 0.20 - 0.60 %
Manganese, Mn 0.90 - 1.4 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.60 %
Zinc, Zn 0.50 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3013-H14 Aluminum
Aluminum 3102-O
Aluminum 3004-O
Alclad Aluminum 3003-H12
Aluminum 3003-O

MA3013 / 9008

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.