MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay CYCOM® 919 Epoxy Prepreg with Graphite Unitape
Categories: Polymer; Thermoset; Epoxy

Material Notes: Property data for specimen with Graphite; Weave style: Unitape; Number of piles: 8.16; Average ply thickness: 0.006 in (0.152 mm); Cure pressure: Autoclave-40 psi (0.27 MPa); Cure temperature: 250°F (121°C); Cure time (cool under pressure): 1 hr; Cure rate per minute: 3.5°F (1.9°C)

CYCOM® 919 is a modified epoxy resin. This resin system offers controlled flow and high elongation permitting direct lamination to honeycomb without the use of additional adhesive. These properties make lightweight sandwich structures possible where impact resistance or a thinner-skin is an important design consideration. Examples include radomes subject to rain erosion and aircraft interiors subject to physical abuse. Other applications are secondary aircraft structure and recreation products. CYCOM 919 composites are serviceable over a temperature range of -67°f to 200°F (-55°C to 93°C) and can be fully cured at 235°F to 260°F (113°C to 127°C) in 60 minutes.

Features & Benefits:

  • Excellent structural properties in solid laminates of moderate thickness
  • Exceptional toughness
  • Controlled flow and high elongation
  • Flame retardant; fire-resistant under FAA-453
  • Serviceable to 200°F (93°C)
  • No post cure required
  • Curing pressures range from 12 psi (0.084 MPa) vacuum to 100 psi (0.70 MPa) positive pressure
  • 20 day out time at room temperature

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 2.5 %2.5 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  1880 MPa
@Temperature -55.0 °C
272000 psi
@Temperature -67.0 °F
 2000 MPa
@Temperature 24.0 °C
290000 psi
@Temperature 75.2 °F
 2050 MPa
@Temperature 71.0 °C,
Time 1800 sec
298000 psi
@Temperature 160 °F,
Time 0.500 hour
Tensile Modulus  133 GPa
@Temperature 24.0 °C
19300 ksi
@Temperature 75.2 °F
 137 GPa
@Temperature -55.0 °C
19900 ksi
@Temperature -67.0 °F
 127 GPa
@Temperature 71.0 °C,
Time 1800 sec
18400 ksi
@Temperature 160 °F,
Time 0.500 hour
Compressive Strength 1613 MPa
@Temperature 24.0 °C
233900 psi
@Temperature 75.2 °F
 1069 MPa
@Temperature 71.0 °C,
Time 1800 sec
155000 psi
@Temperature 160 °F,
Time 0.500 hour
Compressive Modulus 117 GPa
@Temperature 24.0 °C
17000 ksi
@Temperature 75.2 °F
 114 GPa
@Temperature 71.0 °C,
Time 1800 sec
16500 ksi
@Temperature 160 °F,
Time 0.500 hour
Shear Strength 86.2 MPa
@Temperature 24.0 °C
12500 psi
@Temperature 75.2 °F
Interlaminar
 48.3 MPa
@Temperature 71.0 °C,
Time 1800 sec
7000 psi
@Temperature 160 °F,
Time 0.500 hour
Interlaminar
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 113 - 127 °C
@Time 3600 sec
235 - 260 °F
@Time 1.00 hour
Gel Time 4.00 - 12.0 min
@Temperature 121 °C
4.00 - 12.0 min
@Temperature 250 °F
Shelf Life 6.00 Month
@Temperature <=-18.0 °C
6.00 Month
@Temperature <=-0.400 °F
 
Descriptive Properties
Sandwich Peel42 Nm/mNote 1, 42% Resin, 71°C for 30 mins
 47 Nm/mNote 1, 42% Resin, 24°C
 53 Nm/mNote 1, 42% Resin, 93°C for 30 mins
 56 Nm/mNote 2, 42% Resin, 24°C
 58 Nm/mNote 2, 42% Resin, 71°C for 30 mins
 73 Nm/mNote 2, 42% Resin, 93°C for 30 mins
 80 Nm/mNote 2, 42% Resin, 121°C for 30 mins

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 977-3 Neat Epoxy Resin
Solvay CYCOM® 985 Epoxy Neat Resin
Solvay CYCOM® 997 Epoxy Resin
Solvay CYCOM® 7714A Epoxy - Plain Weave (PW) Carbon Fabric Composite
Solvay CYCOM® 7714 Epoxy Resin

PCYTED169_6 / 192691

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.