SABIC® PPcompound 9110 is a talc filled impact modified PP with excellent impact and stiffness ratio. The material exhibits high flow combined with a very high scratch resistance, no stickiness and a low density.
SABIC® PPcompound 9110 designated automotive grade.
IMDS ID: 136528993Information provided by SABIC |