MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Korrobond® 65 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Korrobond® is a two-component epoxy specifically formulated to function as a backing compound in many types of rock crushing equipment. Extensively used within the mining and quarry industry, Korrobond® products have a proven history of quality and reliability worldwide. Korrobond® products are formulated to produce a low viscosity, tough yet flexible backing compound. Korrobond® serves as a backing and reinforcing layer between machine wearing parts as a damper when subject to impact and shock loads. Korrobond 65 is a two-component epoxy backing compound specificallydesigned for various mining and quarrying applications. It serves as a backing and reinforcing layer between machine parts and as a damper when subjected to impact and shock loads.

FEATURES: • Very high compressive strength • 100% Solids, minimal shrinkage • Easy to mix and pour• Long established OEM and after market proven product • High impact strength and resilience.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.6 lb/gal
Viscosity 16000 cP
@Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4000 psiASTM 638
Compressive Strength 17000 psiISO 604
Tensile Impact Strength >= 6.50 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.010 %
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 hour
@Temperature 20.0 °C
Pot Life 15.0 - 20.0 min
@Temperature 20.0 °C
 
Descriptive Properties
ColorLight gray
Lap Shear Strength>353.8 kg
Mix Ratio by volume7 to 1Resin to Hardener
Mix Ratio by weight13.3 to 1Resin to Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWK9046 / 239556

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.