MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Coating P. Materials NB-92A TPU, Injection Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: CPMC has successfully developed a series of products which are suitable for injection types of products and to meet customers’ needs. They all have high abrasion resistance; High tensile strength; High tear strength; Good oil resistance; High transparency CPMC also has all kinds of chemical solvents to provide our customers.

Product Description: Good fluidity, good physical properties, excellent transparency, good abrasion resistance, good flexibility at low temperature

Application To End-Use Products: General extrusion type tube, linear tube, braided hose, coiled tube, reinforced hose, cover on steel wire, wire & cable, profile extrusion. Sealing circle, outsoles and decorations of shoes, parts of sandal, parts of bicycle, sporting equipment, caster roller, dirt-proof boot, mobile phone case, phone keypad, animal ear tags, guide post, top life, gear

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 89 - 9389 - 93ASTM D2240
Tensile Strength 39.2 MPa5690 psiASTM D412
Elongation, Ultimate 700 %700 %ASTM D412
100% Modulus 8.83 MPa1280 psiASTM D412
300% Modulus 18.6 MPa2700 psiASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTCOAT051 / 293995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.