MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV 24378N XRD Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24378N XRD is a high performance thermoplastic vulcanizate used in electrical and industrial applications. This product is a high hardness, high density, flame retardant grade exhibiting superior sunlight resistance. This grade can be processed by injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Brominated; Electrically Insulating; Flame Retardant; Good Colorability; Halogenated; High Density; High Density; High Hardness; High Specific Gravity; Low Flow; Slip; Sunlight Resistant; UV Resistant

Uses: Cable Jacketing; Electrical/Electronic Applications; Industrial Applications; Insulation; Jacketing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
 78
@Time 5.00 sec
78
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 1.38 MPa200 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-2
@Thickness 1.02 mm
V-2
@Thickness 0.0400 in
NC
 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
NC
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 216 - 227 °C420 - 440 °FInjection, Melt
Rear Barrel Temperature 199 - 210 °C390 - 410 °FInjection
Middle Barrel Temperature 204 - 216 °C400 - 420 °FInjection
Front Barrel Temperature 210 - 221 °C410 - 430 °FInjection
Nozzle Temperature 216 - 227 °C420 - 440 °FInjection
Zone 1 193 - 204 °C380 - 400 °FExtrusion
Zone 2 199 - 210 °C390 - 410 °FExtrusion
Zone 3 204 - 216 °C400 - 420 °FExtrusion
Zone 4 204 - 221 °C399 - 430 °FExtrusion
Zone 5 210 - 221 °C410 - 430 °FExtrusion
Die Temperature 216 - 227 °C420 - 440 °FExtrusion
Mold Temperature 35.0 - 65.6 °C95.0 - 150 °FInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceColor Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Elexar® EL-8614A Thermoplastic Elastomer
Envalior Arnitel® PL460-S TPC-ET FR(17), Injection Molding, Flame Retardant
Envalior Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America)
Envalior Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade)

PTEKNQ1186 / 237677

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.