MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 808010 sec; ASTM D2240
Tensile Strength, Yield 42.1 MPa6110 psiType I, 51 mm/min; ASTM D638
Tensile Modulus 2.24 GPa325 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 66.9 MPa9700 psiASTM D790
Flexural Modulus 2.34 GPa339 ksiASTM D790
Izod Impact, Notched 5.30 J/cm
@Temperature -10.0 °C
9.93 ft-lb/in
@Temperature 14.0 °F
Injection Molded; ASTM D256A
 9.60 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
18.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C77.8 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi)  76.1 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
169 °F
@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
 78.9 °C
@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
174 °F
@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  72.8 °C
@Thickness 3.18 mm
163 °F
@Thickness 0.125 in
Compression Molded, Annealed at 50 deg.C; ASTM D648
 77.8 °C
@Thickness 3.18 mm
172 °F
@Thickness 0.125 in
Compression Molded, Annealed at 60 deg.C; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 199 - 210 °C390 - 410 °F
 
Descriptive Properties
AppearanceColors Available
FeaturesHigh Gloss
 High Impact Resistance
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesCapstock
 Construction Applications
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH0POL1227 / 145796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.