MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 2520N Injection Molding Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Impact Copolymer for Injection Molding

Formolene® 2520N is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stability. The improved stiffness and impact balance also provides for utility in industrial applications including bins and crates, and small appliances. Formolene® 2520N meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.

Specimens were injection molded according to the conditions specified in ASTM D4101.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 20 g/10 min
@Temperature 230 °C
I2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psi2" (50mm) per min.; ASTM D638
Elongation at Yield 6.0 %2" (50mm) per min.; ASTM D638
Flexural Modulus, 1% Secant 175000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 2.70 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 2575N injection Molded Polypropylene
Formosa Plastics Formolene® 2610A Compounding and Injection Molding Polypropylene
Formosa Plastics Formolene® 2510A Injection Applications Polypropylene
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene
Formosa Plastics Formolene® 2535A Thin Walled Injection Molding Polypropylene

PFPCPP39_a / 176060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.