MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: 304Cu UGIMA® is an enhanced machining grade, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu UGIMA® also features the added benefit of increased cold formability when compared with that of standard type 304 stainless steels. The increased copper content in 304Cu UGIMA® provides corrosion resistance superior to 304L and comparable to 316L. The unique combination of machinability, cold formability, and corrosion resistance afforded by 304Cu UGIMA® is unique in the industry, and provides the optimum solution for even the most difficult fabrication challenges. 304Cu UGIMA® builds upon the proprietary UGIMA manufacturing process with the addition of copper, allowing for good machinability across a wide range of operations and cutting conditions. It allows for superior machinabilty at both low and high speeds, cam-driven and CNC machines, and with high-speed steel or carbide tooling. Machine shops using 304Cu UGIMA® have experienced consistent success regardless of machine, operation, tooling, or cutting conditions.

Information provided by Schmolz + Bickenbach

Key Words: AISI 304Cu/XM-7; UNS S30430; AMS-QQ-S-763; EN 10088-3 1.4567, X3CrNcUS18-9-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 145 - 185
@Thickness >=25.4 mm
Turned Bars
 180 - 210
@Thickness <=25.4 mm
Cold Drawn Bars
Tensile Strength 70.0 - 90.0 ksi
@Thickness >=25.4 mm
Turned Bars
 85.0 - 105 ksi
@Thickness <=25.4 mm
Cold Drawn Bars
Tensile Strength, Yield 30.0 - 50.0 ksi
@Strain 0.2 %,
Thickness >=25.4 mm
Turned Bars
 70.0 - 90.0 ksi
@Strain 0.2 %,
Thickness <=25.4 mm
Cold Drawn Bars
Elongation at Yield 28 - 40 %
@Thickness <=25.4 mm
Cold Drawn Bars
 48 - 62 %
@Thickness >=25.4 mm
Turned Bars
Reduction of Area 68 - 75 %
@Thickness <=25.4 mm
Cold Drawn Bars
 70 - 82 %
@Thickness >=25.4 mm
Turned Bars
Tensile Modulus 29000 ksi
@Temperature 20.0 °C
 29000 ksi
@Temperature 500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µin/in-°F
@Temperature 20.0 - 500 °C
 9.17 µin/in-°F
@Temperature 20.0 - 200 °C
Thermal Conductivity 116 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
 125 BTU-in/hr-ft²-°F
@Temperature 500 °C
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature >= 1750 °FForge
 1830 - 2190 °FForging range
 2100 - 2230 °FHeat in range
 <= 2350 °FHeat of core during fast forging
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 17 - 19 %
Copper, Cu 3.0 - 4.0 %
Iron, Fe >= 63.825 %
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 10 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
 
Descriptive Properties
Corrosion ResistanceAcetic Acid2/4
 Humidity4/4
 NaCl (Saline Mist)3/4
 Nitric Acid2/4
 Petroleum2/4
 Phosphoric Acid3/4
 Sodium Carbonate2/4
 Sulfuric Acid3/4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 4567 Austenitic Stainless Steel
AK Steel 316 Austenitic Stainless steel
AISI 302Cu Stainless Steel soft tempered 2.54- 25.4 mm diameter wire
AISI 304 Cast Stainless Steel, SUS304
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar

NSCHMO035 / 125908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.