MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Orion Engineered Carbons CORAX® N 330 ASTM Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Standard grade of furnace black in accordance with the requirements of ASTM D 1765

Hard Black - tread grade, reinforcing carbon black

Information provided by Orion Engineered Carbons.

Key Words: ASTM D 1765; Hard Black
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.370 g/ccPour Density; ASTM D 1513
Oil Absorption 88 %(ml/100 g); Compressed Sample; ASTM D 3493
 102 %(ml/100 g); ASTM D 2414
Loss On Ignition <= 1.0 %Heating Loss; ASTM D 1509
Specific Surface Area 76 m²/gStatistical thickness surface area; ASTM D 6556
Iodine Absorption Number 82mg/g; ASTM D 1510
 
Descriptive Properties
Fines< 7.0 %ASTM D 1508
Individual Pellet Hardness< 45 gASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue< 500 ppmASTM D 1514
Tint103ASTM D 3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Orion Engineered Carbons CORAX® N 339 ASTM Carbon Black
Orion Engineered Carbons CORAX® N 220 ASTM Carbon Black
Orion Engineered Carbons CORAX® N 115 ASTM Carbon Black
Orion Engineered Carbons CORAX® N 121 ASTM Carbon Black
Orion Engineered Carbons CORAX® N 134 ASTM Carbon Black

EORION907 / 159731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.