MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® Ultraflow K-FHG0 PA6-GF50, Dry, 50% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: 50% Glass Reinforced, Heat Stabilized, High Flow

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Water Absorption 4.5 %Sim. ISO 62
Moisture Absorption 1.40 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 220 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 16500 MPaISO 527-1/-2
Flexural Strength 335 MPaISO 178
Flexural Modulus 15500 MPaISO 178
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.5
@Frequency 100 Hz
IEC 60250
 5.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°CISO 11359-1/-2
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
Glow Wire Flammability Index 800 °C
@Thickness 3.10 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow K-FHG0 PA6-GF50, Conditioned, 50% Glass Filled, Heat Stabilized
Envalior Akulon® Ultraflow K-FHG6 PA6-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Dry, 30% Glass Filled, High Flow
Envalior Akulon® Ultraflow K-FHG12 PA6, Dry-GF60, 60% Glass Filled, Heat Stabilized
BASF Ultramid® A3WG6 HRX BK 23591 30% Glass Filled PA66 (Conditioned)

PDSM8085 / 184786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.