MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Geniosil® GF 96 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C6H17NO3Si

CAS No.: 13822-56-5

Properties: In addition to its application as an adhesion promoter in formulations and primers, GENIOSIL® GF 96 functions as a surface modifier in fillers and pigments, where it improves the dispersibility of the filler and the mechanical properties - such as flexural strength, tensile strength and modulus - of the composites. The silane also reduces the filler's sedimentation tendency in the uncured polymer. GENIOSIL® GF 96 also greatly increases water (vapor) and corrosion resistance.

Special features: GENIOSIL® GF 96 is an alkoxysilane with an aminofunctional group. It´s a clear, colorless liquid with a characteristic amine odor. As a bifunctional amine, GENIOSIL® GF 96 can also interact with numerous organic polymers and thus function as a molecular bridge between organic and inorganic substrates.

Application: GENIOSIL® GF 96 is used mainly as an adhesion promoter in sealants, adhesives and coatings, and as a surface modifier for fillers (e.g. glass, mineral wool, mica, metal oxides) and pigments used in various plastics, including epoxy resins, polyamides, polyacrylates, polyurethanes, ethyl/vinyl acetate polymers and phenolic resins.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.014 g/cc
Viscosity 1.6 cPDIN 51562-1
Molecular Weight 179.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 210 °C
Flash Point 79.0 °CEN 22719
Ignition Temperature 300 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.424
 
Descriptive Properties
Amine number5.5
Purity>95%GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dymax 3073 Solvent-Free Plastic Adhesive
Dow Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
Silon Tabond 2001 Adhesive Resin
LyondellBasell Plexar® PX3410 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE

PWACK9323 / 204852

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.