This Carbon Graphite Ink is designed to be used for screen printing working electrodes. These electrodes enable the detection of many analytes when used in conjunction with peroxidase and other oxidase type enzymes. The ink contains Potassium Ferrocyanide a mediator that makes the electrodes suitable to use with Horseradish Peroxidase for hydrogen peroxide (H2O2) detection. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156-230tpi Substrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd. |