MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.

Application Information: TECKNIT WAVEGUIDE GASKETS offer the circuit designer a wide variety of RF and pressure tight seals for any waveguide system. They can be used for EMP and TEMPEST applications, and are widely used by the military and aerospace communities in sophisticated electronic countermeasure, communication, and guidance systems.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.045 - 3.955 g/cc3.045 - 3.955 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 8773 - 87ASTM D2240
Tensile Strength 2.76 MPa400 psiASTM D412
Elongation at Break 100 - 300 %100 - 300 %ASTM D412
Tear Strength 7.01 kN/m40.0 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0050 ohm-cm<= 0.0050 ohm-cmQA-1039
Shielding Effectiveness  75 dB
@Frequency 100000 Hz
75 dB
@Frequency 100000 Hz
H-Field
 110 dB
@Frequency 1e+10 Hz
110 dB
@Frequency 1e+10 Hz
Plane Wave
 115 dB
@Frequency 1e+9 Hz
115 dB
@Frequency 1e+9 Hz
Plane Wave
 >= 130 dB
@Frequency 1e+7 Hz
>= 130 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
 
Descriptive Properties
ConsistencySmooth
ElastomerSilicone
FillerSilver Plated Copper Particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Silicone Polyurethane, Polycarbonate Based
Overview of materials for Silicone Polyurethane, Ether Based
Overview of materials for Liquid Silicone Rubber

PCHOME420 / 131130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.