MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt HUP 31838/30 RN-1090 Aircraft Homologate
Categories: Polymer; Thermoset; Polyester, TS

Material Notes:

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183 A
Filler Content 30 %30 %Fiber; ISO 1172
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 150 MPa21800 psiISO 14125
Flexural Modulus 8.00 GPa1160 ksiISO 14125
Tensile Impact Strength 65.0 kJ/m²30.9 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 93
Dielectric Strength >= 10.0 kV/mm>= 254 kV/inIEC 243-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FIEC 60216
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 140 - 150 °C284 - 302 °F
Hold Pressure 8.00 - 12.0 MPa1160 - 1740 psiMolding pressure
Cure Time 1.83 min0.0306 hourISO 12114/1
 
Descriptive Properties
Fiber length25 mmDF PA3.01
Molding time> 25 sec./mm
Surface Weight3000 g/m2ISO 10352
Water Absorption<50 mgISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9035 / 231630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.