MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Water Absorption 0.30 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 5.5 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75ASTM D785
Tensile Strength 13500 psiASTM D638
Tensile Strength at 65°C (150°F) 6000 psiASTM D638
Elongation at Break 5.0 %ASTM D638
Tensile Modulus 675 ksiASTM D638
Flexural Strength 21000 psiASTM D790
Flexural Modulus 650 ksiASTM D790
Compressive Strength 18000 psi10% Def.; ASTM D695
Compressive Modulus 600000 psiASTM D695
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+13 ohmEOS/ESD S11.11
Dielectric Strength 350 V/milShort Term; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 1.70 BTU-in/hr-ft²-°FASTM F433
Melting Point 500 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 220 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 400 °FASTM D648
Flammability, UL94 V-2
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
Machinability41-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 H. S. Type 6 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® MC® 907 PA6 Natural and Black, Unfilled Type 6 nylon (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet)
Overview of materials for Polycarbonate, Molded

P1SM21A / 20105

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.