MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 104 H Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, Impact Grade

Material Notes: Availability: Europe; Asia Pacific; North America

Additive: Heat Stabilizer; Impact Modifier

Features: General Purpose; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Impact Modified

Automotive Specifications: CHRYSLER MS-DB-41 CPN3955 Color: NT001 Natural; CHRYSLER MS-DB-41 Type PA CPN1826 Color: BK001 Black; FORD ESA-M4D267-A; FORD ESA-M4D387-A; FORD ESB-M4D178-A2; FORD ESK-M4D178-A2; FORD WSB-M4D706-A; FORD WSB-M4D706-A2; FORD WSK-M4D706-A; FORD WSK-M4D706-A2; FORD WSS-M4D706-B1; GM GMP.PA66.015 Color: Natural; GM GMW16447P-PA66-T2

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792
Water Absorption 0.90 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.012 - 0.020 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 9000 psiASTM D638
Elongation at Break 35 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Strength 10500 psiASTM D790
Flexural Modulus 330000 psiASTM D790
Izod Impact, Notched 2.60 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 4.50 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 430 V/mil
@Thickness 3.00 mm
ASTM D149
Comparative Tracking Index 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 39.0 µin/in-°FASTM D969
Deflection Temperature at 0.46 MPa (66 psi) 415 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 175 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.762 mm
Oxygen Index 22 %ASTM 2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 465 - 490 °F
Middle Barrel Temperature 495 - 525 °F
Front Barrel Temperature 505 - 535 °F
Nozzle Temperature 505 - 535 °F
Melt Temperature 495 °F
 505 - 535 °F
Drying Temperature 175 °F
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
DuPont Mobility and Materials Zytel® 42A NC010 PA66
Envalior Akulon® K223-TP4 PA6-I, Dry, Impact Modified
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Conditioned)

PTEKNQ0431 / 236922

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.