MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Coating P. Materials ER-8315S TPU, Polyether Type
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: TPU extrusion series are commonly applied to extrusion products: Excellent abrasion resistance; Good temperature resistance; Slice resistance; Tear resistance; Break-stretching resistance; Easy to process; Light and transparent; Practical and pleasing to the eyes

Product Description: Good flexibility at low temperature, hydrolysis resistance, fungus resistance, good fluidity

Application To End-Use Products: General extrusion type tube, linear tube, fire hose, coiled tube. Reinforced hose, cover on steel wire, wire and cable, profile extrusion

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83 - 87ASTM D2240
Tensile Strength 320 kg(f)/cm²ASTM D412
Elongation, Ultimate 500 %ASTM D412
100% Modulus 70.0 kg(f)/cm²ASTM D412
300% Modulus 170 kg(f)/cm²ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCOAT101 / 294045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.