MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals NOVAPOL® LF-Y824-C LDPE Clarity Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes:

Homopolymer

Features:

  • Good optical clarity
  • Excellent shrink film characteristics

Additive Packages:

  • Antiblock (1200 ppm)

Applications:

  • Clarity shrink film
  • Produce and bakery film
  • Textile packaging film

Film properties are typical of blown film extruded on a 1.5" extruder with 3" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL LF-Y824-C resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.2, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D 792
Thickness 38.0 microns1.50 mil
Melt Index of Compound 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.0 MPa2030 psiASTM D 882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D 882
Film Elongation at Break, MD 290 %290 %ASTM D 882
Film Elongation at Break, TD 520 %520 %ASTM D 882
Elmendorf Tear Strength MD 195 g195 gASTM D 1922
Elmendorf Tear Strength TD 245 g245 gASTM D 1922
Dart Drop Test 130 g0.287 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 23.0 MPa3340 psiASTM D 882
Film Tensile Strength at Break, TD 18.0 MPa2610 psiASTM D 882
1% Secant Modulus, MD 190 MPa27600 psiASTM D 882
1% Secant Modulus, TD 210 MPa30500 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %6.0 %ASTM D 1003
Gloss 70 %70 %@ 45°; ASTM D 2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)13NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVB024 / 194632

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.