MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80ASTM D785
Tensile Strength, Yield 3200 psi2 in/min; ASTM D638
Flexural Modulus 155 ksi0.5 in/min, Tangent Method; ASTM D790
Izod Impact, Notched 0.700 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 1.50 ft-lb/in
@Temperature 0.000 °C
ASTM D256
 NB
@Temperature 22.8 °C
ASTM D256
Falling Dart Impact 20.8 ft-lb
@Temperature -30.0 °C
0.5" Tup, 150"/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 175 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HH450MO Polypropylene
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
Braskem H362-09RS Cast Film Polypropylene
Aclo Accutech Polypropylene Homopolymer HP0339C30L1 Calcium Reinforced
Overview of materials for Polypropylene with 50% Glass Fiber Filler

PATOP029 / 79972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.