MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 155 Solvent-Based Battery Fabrication Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Low fuming
  • Minimal residue
  • Not highly corrosive to equipment
  • Free of chlorides
  • Free of organic acids
  • Rapid evaporation of solvent
  • Wide window of operating temperatures
Description: Superior No. 155 Solvent Base Battery Flux was specially formulated for high-volume case-on-strap manufacturing operations where rapid evaporation of solvent is necessary. The flux contains no chlorides, heavy metals or organic acids that could affect the long-term life of the batteries. Other key advantages are the wide window of operation at various temperatures and line speeds. Whether operating at low temperatures due to straps cracking or high temperatures to accommodate the large mass plates, Superior No. 155 remains consistently active to produce strong burn-in cast bonds.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.046 g/cc1.046 g/cc
Density 1.04 g/cc0.0377 lb/in³
 
Thermal PropertiesMetricEnglishComments
Flash Point 29.0 °C84.2 °FTCC Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 455 °C500 - 851 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
AppearanceClear Liquid
ColorRed
Conductivity350-450 Mv

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, General Purpose
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose
Ascend Performance Materials Vydyne® 21SPC Nylon 66, General Purpose

NSFLUX049 / 185733

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.