Parcolene 99X post-treatment is a chromium- and phosphate-free post-treatment especially formulated for use over all types of conversion coatings used in the pretreatment of steel, zinc and aluminum surfaces. Application: Zinc Phosphate Conversion Coating |
Aerospace Surface Treatment |