MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel - Easy Processing - Good Melt Strength - Soft Touch

Color concentrates with ethylene vinyl acetate (EVA) carriers are most suitable for coloring Dynaflex™ D3202-1000-03. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow rate of 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. A high color match consistency may be obtained by using precolored compounds available from GLS. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 200 to 800 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 3 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.988 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cmASTM D955
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 59 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5910 sec; ASTM D2240
Tensile Strength at Break 4.48 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 4.62 MPa
@Strain 100 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 230 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 24.5 kN/mASTM D624
Compression Set 16 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 116 - 171 °C
Middle Barrel Temperature 166 - 188 °C
Front Barrel Temperature 177 - 204 °C
Nozzle Temperature 177 - 204 °C
Mold Temperature 21.1 - 32.2 °C
Back Pressure 0.000 - 0.758 MPa
Screw Speed 40 - 100 rpm
 
Compliance PropertiesOriginal ValueComments
FDA YesUnspecified Rating
 
Descriptive Properties
AppearanceNatural Color
FeaturesGood Melt Strength
 Good Processability
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesConsumer Applications
 General Purpose
 Toys

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)

PH0POL0029 / 144598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.