MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Shinil Chemical SHINFLAME PA-66 GF Flame Retardant Polymer Under Hood
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to produce high performance SHINFLAME compound. SHINFLAME compounds comprise halogen or non halogen flame retardant additives in engineering thermoplastics. SHINFLAME provides a wide range of the flame performance (V0, V1, V2, HB etc), mechanical and physical properties to create the application-specific environment.

    Feature and Benefits
  • Excellent fire performance
  • Non halogen FR available
  • Environmentally friendly
  • RoHS compliance (selected grade)
  • Outstanding mechanical properties
  • Improved thermal properties
  • Easy processing
  • Non toxic

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1150 kg(f)/cm²
Elongation at Break 4.0 %
Flexural Strength 196.2 MPa
Flexural Modulus 85000 kg(f)/cm²
Izod Impact, Notched 7.00 kg-cm/cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
PTS Trimid® N6-TG30L-BK 30% Glass Fiber, High Impact Nylon 6
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced
Mitsubishi Chemical Advanced Materials Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)

PSHINL35 / 104037

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.