MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Features

Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properties, these can be modified by addition of GF, as a result of which the anisotropy worsens.PA 6 for injection moulding, reinforced with 20% glass beads offers high grade surface brightness, low rolling resistance force. Application: eg. throttle valves for air piping. Delivered in natural mode and in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/cc
Viscosity Measurement 1.54 - 1.62
Linear Mold Shrinkage 0.0154 cm/cm
Linear Mold Shrinkage, Transverse 0.0162 cm/cm
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa
Elongation at Break 20 %
Tensile Modulus 3300 MPa
Flexural Strength 85.0 MPa
Flexural Modulus 2800 MPa
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
 45.0 kJ/m²
@Temperature -20.0 °C
Charpy Impact, Notched 1.50 kJ/m²
@Temperature -20.0 °C
 2.50 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
Vicat Softening Point 200 °CB
Flammability, UL94 HB
Glow Wire Test 650 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 100 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 20 LS PA6, 20% glass beads, light stability
Plastcom SLOVAMID 6 CF 20 PA6, 20% carbon fibre
Polyram PlusTek PB340S6 Nylon 6, 30% Glass beads
Plastcom SLOVALEN PQ 81 T 10 PP, 10% mineral filling
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre

PPLACO321 / 120945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.