MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman Benzoflex™ 2-45 Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Benzoflex™ 2-45 is also compatible with, and an excellent solvator for, polyvinyl chloride (PVC). Flexible vinyl formulations based on this plasticizer can be processed quicker and/or at lower temperatures than vinyls based on a di-2-ethylhexyl phthalate. Benzoflex™ 2-45 is also resistant to extraction from the vinyl by aliphatic and oily solvents.

Application/Uses:

  • Flexible PVC
  • PVC plastisols

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³
Viscosity 74 cP74 cP
Vapor Pressure 0.00000122 bar0.000912 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 16.0 - 28.0 °C60.8 - 82.4 °FFreezing Point; Two crystal forms
Boiling Point >= 300 °C>= 572 °F
Flash Point 194 °C381 °FSetaflash Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54
 
Descriptive Properties
Acidity<0.1%
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 8863 Moldings & Extrusions Flexible PVC
Colorite Polymers 2019F Rigid PVC
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride
Teknor Apex Sinvicomp SFE 5000 Polyvinyl Chloride, Flexible
Vycom Corzan® CPVC Chlorinated PVC

PEATM5068 / 222262

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.