MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum K12® Dual Hardness Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.

The composition of both faces is a Ni-Mo-Cr steel, but the front side has a higher carbon content, which leads to a higher hardness after heat treatment. The front and back sides are roll bonded by a multi-step, proprietary process which involves heating the assembly to a specific temperature and hot rolling it until the two sides develop a strong, metallurgical bond. The roll-bonded plates are annealed, sheared, and flattened. A careful and precise heat treatment is required to achieve optimum ballistics performance.

Information provided by Allegheny Ludlum.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 233 - 286Annealed; Soft Side
 293Annealed; Hard Side
Hardness, Rockwell C 48 - 54Heat Treated; Soft Side
 58 - 64Heat Treated; Hard Side
Tensile Strength, Ultimate 148000 psiAverage Annealed
Tensile Strength, Yield 130000 psi
@Strain 0.2 %
Elongation at Break 14.5 %Average Annealed
Compressive Yield Strength 234000 psi0.2%; Average Transverse Hardened
 238000 psi0.2%; Average Longitudinal Hardened
Charpy Impact 12.0 - 13.0 ft-lb0.009" V-Notch in soft side; struck on hard side; Heat Treated
Charpy Impact, Unnotched 154 ft-lbHeat Treated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000260 ohm-cm
@Temperature 0.000 °C
 0.0000310 ohm-cm
@Temperature 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 21.0 - 93.0 °C
Specific Heat Capacity 0.481 J/g-°C
@Temperature 21.0 - 93.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
301 Stainless Steel

NLK12 / 18007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.