MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman 1924P Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, ease of processing, good chill-roll release, low coefficient of friction (for ease of indexing carton blanks) and good heat sealability. It is characterized by high-speed processability, excellent drawdown and reliable lot-to-lot consistency.

List of Applications:

  • Food-contact applications
  • Photographic paper

Information supplied by the manufacturer.

Information from manufacturer data sheet.

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Key Words: Low neck-in, ease of processing, good chill-roll release, low coefficient of friction and good heat sealability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D4883
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 10.0 MPa500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 14.0 MPa500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 100 %500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.310 GPa
@Strain 2 %
Secant; 12.7 mm/min. (0.5 in./min.); ASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °CASTM D1525
Brittleness Temperature -58.0 °CASTM D746
 
Descriptive Properties
ProcessCoating

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical PA828 Processing aid
Ineos R08S-00 Polypropylene Random Copolymer
3M Dyneon™ FX 5929 Polymer Processing Additive
3M Dyneon™ Dynamar™ FX 5927 Polymer Processing Additive
Shandong Rike Chemical HELI™ HL-220N PVC Processing Aid Series (PA)

PEAT280 / 35365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.