MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MOCOM (ALBIS) Cellidor® B 500-05 Cellulose Acetate Butyrate
Categories: Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Base Polymer: Cellulose Acetate Butyrate

Filler/Additive System: 5% phthalate-free plasticizer

Special Features: Low odor

Typical Applications: Various

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Time 86400 sec
0.0040 - 0.0070 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 410 °F
cm3/10min, volumetric value; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 90.0 MPa13100 psiH132/30; ISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psiISO 527-1/-2
Tensile Strength, Yield 50.0 MPa7250 psiISO 527-1/-2
Elongation at Break 10 %10 %ISO 527-1/-2
Elongation at Yield 4.7 %4.7 %ISO 527-1/-2
Tensile Modulus 2.00 GPa290 ksiISO 527-1/-2
Flexural Strength 60.0 MPa8700 psi3.5% flexural stress; ISO 178
Charpy Impact Unnotched 11.5 J/cm²54.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1/-2
Vicat Softening Point 100 °C212 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 230 °C356 - 446 °Finjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °Finjection molding
Drying Temperature 60.0 - 90.0 °C
@Time 7200 - 14400 sec
140 - 194 °F
@Time 2.00 - 4.00 hour
in air circulating dryer, dependant on moisture content
Moisture Content <= 0.0015 %<= 0.0015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay GEROPON® SDS Surfactant
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Evonik TEGOSTAB® B 4113
Eastman Cristal™ 10101 Microfiber
Arkema Evatane® 1005 VN 2 Ethylene Vinyl Acetate

PALBIS9918 / 221014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.