MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton MRS 10 Metal Rebuilding System
Categories: Ceramic

Material Notes: Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 100% solids. The MRS 10 is formulated for applications where machining to exact tolerance is required or desired. It is frequently used as an alternative to resurfacing by welding or flame spraying. MRS 10 is easily mixed and applied and cures without the need of heat or pressure.

Benefits:

  • High build characteristics allows for single coat applications
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance
  • Can be easily machined to exact tolerance.
  • Convenient 4-1 mix ratio and verification of mix by color change
  • Performs well under fluctuating chemical environments
  • Resists compression setting.

Suggested Uses:

  • Condensers
  • Cooling Water Pumps
  • Flange Faces
  • Hydraulic Rams
  • Keyways
  • Valve Bodies
  • Bearing Housings
  • Shafts
  • Spline Repairs
  • Pitted Castings
  • Heat Exchangers
  • Pump Volutes

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Hardness, Shore D 8686ASTM D2240
Tensile Strength at Break 27.6 MPa4000 psiASTM D638
Flexural Strength 68.9 MPa10000 psiASTM D790
Flexural Modulus 3.52 GPa510 ksiASTM D790
Compressive Strength 89.6 MPa13000 psiASTM D695
Taber Abrasion, mg/1000 Cycles 275
@Load 0.250 kg
275
@Load 0.551 lb
H-18, loss; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °FWet
 93.0 °C199 °FDry
 
Processing PropertiesMetricEnglishComments
Cure Time  150 min
@Temperature 32.0 °C
2.50 hour
@Temperature 89.6 °F
Light Load
 210 min
@Temperature 25.0 °C
3.50 hour
@Temperature 77.0 °F
Light Load
 420 min
@Temperature 16.0 °C
7.00 hour
@Temperature 60.8 °F
Light Load
 540 min
@Temperature 10.0 °C
9.00 hour
@Temperature 50.0 °F
Light Load
 960 min
@Temperature 32.0 °C
16.0 hour
@Temperature 89.6 °F
Full Load
 1200 min
@Temperature 25.0 °C
20.0 hour
@Temperature 77.0 °F
Full Load
 1800 min
@Temperature 32.0 °C
30.0 hour
@Temperature 89.6 °F
Full Chemical
 2160 min
@Temperature 16.0 °C
36.0 hour
@Temperature 60.8 °F
Full Load
 2160 min
@Temperature 25.0 °C
36.0 hour
@Temperature 77.0 °F
Full Chemical
 2880 min
@Temperature 10.0 °C
48.0 hour
@Temperature 50.0 °F
Full Load
 4320 min
@Temperature 16.0 °C
72.0 hour
@Temperature 60.8 °F
Full Chemical
 5760 min
@Temperature 10.0 °C
96.0 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  60.0 min
@Temperature 32.0 °C
1.00 hour
@Temperature 89.6 °F
 120 min
@Temperature 25.0 °C
2.00 hour
@Temperature 77.0 °F
 180 min
@Temperature 16.0 °C
3.00 hour
@Temperature 60.8 °F
 300 min
@Temperature 10.0 °C
5.00 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
Chesterton 218 HDP Liquid alkaline degreaser
Chromium Nitride (CrN) PVD Coating

PPTCHS128 / 138240

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.