MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3D IND402™ A70 High Rebound Black Elastomeric UV Photocurable Resin
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset

Material Notes: Henkel® Loctite® IND402 is a single-component elastomer material with high elongation and resilience, excellent tensile strength, and high energy return. Parts can be printed on various Digital Light Processing (DLP) and Continuous Digital Light Manufacturing (cDLM) systems and do not require thermal post-processing. Loctite Engineering Grade products are high-performance fluids developed to be highly consistent with extraordinary attributes. This elastomeric UV photocurable resin exhibits high resilience while maintaining excellent tensile strength. E-IND402 is a single-component system with excellent green strength and does not require thermal post-processing.

Applications: consumer products, sportswear, automotive, industrial.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccLiquid
 1.10 g/ccASTM D1475
Water Absorption 3.15 %
@Time 86400 sec
ASTM D570
Viscosity 13500 cPLiquid as Supplied
 6000 cP
@Temperature 40.0 °C
Liquid as Supplied
 8400 cP
@Temperature 35.0 °C
Liquid as Supplied
 14500 cP
@Temperature 25.0 °C
Liquid as Supplied
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73.0
@Time 3.00 sec
ASTM D648
Tensile Strength at Break 1.99 - 2.61 MPaGreen; ASTM D638
 1.90 MPa
@Temperature 100 °C
Post-processed; ASTM D412
 3.30 MPa
@Temperature 40.0 °C
Post-processed; ASTM D412
 12.0 MPa
@Temperature -20.0 °C
Post-processed; ASTM D412
Tensile Strength 5.50 - 5.70 MPaASTM D638
Tensile Stress at Strain 3.00 - 3.50 MPa
@Strain 50 %
Post-processed; ASTM D412
 3.40 - 4.00 MPa
@Strain 100 %
Post-processed; ASTM D412
 4.00 - 4.60 MPa
@Strain 150 %
Post-processed; ASTM D412
Elongation at Break 132 - 220 %Green; ASTM D638
 220 - 240 %Post-processed; ASTM D638
 260 - 295 %Post-processed; ASTM D412
 279 - 291 %ASTM D638
 285 %
 80.0 %
@Temperature 100 °C
Post-processed; ASTM D412
 140 %
@Temperature 40.0 °C
Post-processed; ASTM D412
 290 %
@Temperature -20.0 °C
Post-processed; ASTM D412
Modulus of Elasticity 0.0300 GPa
 0.0250 - 0.0350 GPaASTM D638
 13.0 - 17.0 GPagreen; ASTM D638
 37.0 - 47.0 GPapost-processed; ASTM D638
Tear Strength 27.0 - 29.0 kN/mpost-processed; ASTM D624
Compression Set 57.1 %
@Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
CTE, linear 187.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Glass Transition Temp, Tg -66.0 °CASTM E1356
 
Descriptive Properties
Appearance as SuppliedSelf leveling, Newtonian red fluid
ColorBlack, gray
Energy Return (%)37Internal Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT00_j / 305370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.