MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Acrylic (PMMA); Vinyl (PVC); PVC/Acrylic Alloy

Material Notes: Utility grade

Applications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.

Features: Vinyloy 100 sheet is a recycled grade of proprietary acrylic/PVC thermoplastic sheet that is cost competitive with other utility grades of thermoplastic sheet while offering improved performance. Vinyloy 100 sheet is UL recognized 94 V-0 and 5V.

Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.

Data provided by the Kleerdex Company.

Kleerdex Company became KYDEX, LLC in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 88ASTM D785
Tensile Strength, Ultimate 42.0 MPaASTM D638
Modulus of Elasticity 2.068 GPa
Flexural Yield Strength 63.0 MPaASTM D790
Izod Impact, Notched 4.27 J/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °Cannealed; ASTM D648
Flammability, UL94 V-0V-0, 5V; UL Standard 94
 
Processing PropertiesOriginal ValueComments
Processing Temperature 162 - 200 °CForming Temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 5555 Acrylic/PVC
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
Chi Mei Polylac® PA-765 ABS - Flame Retardant
Asahi Kasei DELPET™ PM120N Acrylic (PMMA), Heat Resistant
RTP Company RTP 1800 A FR UV Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - UV Stabilized

PKLEER22 / 48875

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.