MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives SONLOCK™ 3510 Anaerobic Gasket Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: SONLOK 3510 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting metal surfaces. SONLOK 3510 is a high temperature resistance gasketing sealant with excellent chemical resistance.

Applications:

  • Used as a form-in-place gasket on flanged connections.
  • Typical uses are engine casings and gearbox.
  • Thixotropic nature reduces the migration of liquid product after application.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 188000 - 500000 cPThixotropic, RVT, Spindle 7 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1085 psiSteel, grit blasted; ISO 6922
Compressive Strength >= 1085 psi
@Time 86400 sec
Steel Pins & Collars; ISO 10123
Shear Strength 725 psiSteel, grit based; ISO 4587
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -65.0 °F
Flash Point >= 93.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 4.00 hourHandling, Primed Surfaces
 2.00 - 8.00 hourHandling, Unprimed Surfaces
 
Descriptive Properties
ColorRed
CompositionDimethacrylate ester
Diameter<0.2 mmThread/Gap Filling
Initial Strength Retained (%)100Acetone for 500 hrs at 22°C
 100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 110Water/Glycol for 500 hrs at 87°C
 110Water/Glycol for 1000 hrs at 87°C
 75Gasoline for 500 hrs at 22°C
 75Gasoline for 1000 hrs at 22°C
 85Ethanol for 1000 hrs at 22°C
 90Ethanol for 500 hrs at 22°C
 95Break Fluid for 500 hrs at 22°C
 95Break Fluid for 1000 hrs at 22°C
 95Acetone for 1000 hrs at 22°C
Solvent ContentNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN029 / 186472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.