Yttria-Tetragonal Zirconia Polycrystal (Y-TZP) with excellent transformation toughening properties. Comprising 3 mol% (5.2 wt%) Y2O3 in ZrO2. A high purity, fine grain (sub-micron) tetragonal, transformation toughened zirconia (3Y-TZP). Prime Features: - Very high mechanical strength
- Excellent wear and abrasion resistance
- High impact resistance and toughness
- Good thermal shock resistance
Typical Applications: - Typically used for blades and cutting edges where the fine grain structure is an advantageous
- Gas and Oil field applications
- Pump and Valve components
- Canning and Metal Packaging
- Solids Handling. Automotive (eg Weld Pins)
Production Capabilities:- Sintered components
- Precision ground components
- Ceramic / Metal assemblies
- Ceramic design assistance
Information provided by Morgan Advanced Materials |